How to hard oxidize aluminum parts
Release time:
2021-02-20 14:22
Hard anodizing stands for hard anodizing. Generally, the thickness of 25-150um is required. The thickness of most hard anodized films is 50-80um, and the thickness of hard anodized films is less than 25um. The parts are used in occasions such as tooth keys, spirals, wear resistance or insulation. Under the process conditions, it is required to produce a hard anodic oxide film with a thickness greater than 125um, but it must be noted that the thicker the anodic oxide film thickness, the lower the microhardness of the outer layer and the greater the surface roughness of the film.
The hard anodizing bath is generally a sulfuric acid solution, and there are also organic acids added with sulfuric acid, such as oxalic acid and sulfamic acid. In addition, hard anodizing can be achieved by reducing the oxidation temperature and sulfuric acid concentration. For copper content exceeding 5% or silicon content exceeding 8% or high silicon die-cast aluminum parts, some special measures for anodizing may also be considered.
For example, 2XXX series aluminum alloys, in order to avoid aluminum parts burning during anodization, 385g/L sulfuric acid and 15g/L oxalic acid can be used as electrolyte, and the current density should also be increased to 2.5A/dm.
Hard oxidation process of aluminum parts:
There are many methods for hard anodizing of electrolytic aluminum parts, such as sulfuric acid, oxalic acid, propylene glycol, sulfosalicylic acid and other inorganic salts and organic acids. The power supply can be divided into several types such as DC, AC, AC and DC stacking, pulse stacking, etc. The following types of hard anodizing power supplies are widely used.
(1) Hard sulfuric acid anodizing method;
2. Oxalic acid hard anodizing method.
3. Mixed acid type hard anodizing.
According to the editor of Transit Aluminum, among these methods, the sulfuric acid method is a widely used hard oxidation method for aluminum parts.
Previous Page