Aluminum extrusion process
Release time:
2021-02-20 14:42
Aluminum extrusion molding is mainly divided into: three temperatures, extrusion speed, tractor speed, extrusion rod speed, quenching, annealing
In order to improve the production efficiency of aluminum extrusion, good equipment is also the key, especially the three major parts of aluminum extrusion press, aluminum rod heating furnace, and mold heating furnace. The most important thing is to have a good extrusion workshop. And aluminum alloy processing.
Tractor speed
The speed of the tractor is an important indicator of production efficiency. However, different profiles, shapes, alloys, sizes, etc. may affect the speed of the tractor. Solid cannot be generalized. Modern Western extrusion plants can achieve a tractor speed of 80 meters per minute.
Extrusion rod speed The extrusion rod speed is another important indicator of productivity. It is measured in millimeters per minute or per minute. When studying production efficiency, the speed of the extrusion rod is often more reliable than the speed of the tractor, because different profiles, shapes, alloys, sizes, etc. may affect the speed of the tractor.
Die Oven Die Oven The die temperature is very important to the quality of the extruded profile. The die temperature must be kept at about 426°C before extrusion. Otherwise, it will easily cause blockage or even damage to the mold. The temperature of the container The temperature of the container must be kept at about 426°C. Quenching temperature (temperature difference) The purpose of quenching (cooling) is to "freeze" the alloying elements, namely magnesium and, to stabilize the unstable magnesium and (silicon) atoms without allowing them to precipitate. To maintain the strength of the profile.
The three main quenching methods include: Air cooling, water mist cooling, and water tank cooling. Which quenching method is used depends on the extrusion speed, profile thickness and required physical properties, especially the strength requirements. Alloy type The alloy type is a comprehensive indication of the hardness and elastic properties of the alloy. The Aluminum Association of the United States has detailed regulations on the aluminum alloy type: The basic state code The basic state code of aluminum, magnesium and its alloys is: F Free processing state, It is suitable for products that do not have special control over the temperature or the degree of work hardening of the material during the molding process (no mechanical performance requirements for processed products);
O annealed state, suitable for processed products with the lowest strength after annealing and cast products with improved ductility and ruler stability after annealing. O can be suffixed with an Arabic numeral other than zero; H work-hardened state, suitable for passing Work hardening products to increase strength (this product can be heat treated to reduce some strength), H is always suffixed with more than two Arabic numerals;
Previous Page
Previous Page
Related News